Journal of Applied Physics

Nitrogen related paramagnetic defects: Decoherence source of ensemble of NV− center

Chikara Shinei, Y. MASUYAMA, Masashi Miyakawa, Hiroshi Abe, Shuya Ishii, Seiichi Saiki, Shinobu Onoda, Takashi Taniguchi, Takeshi Ohshima, Tokuyuki Teraji

Published Dec 7, 2022• 32 citations
Publisher

Abstract

We investigated spin-echo coherence times T2 of negatively charged nitrogen vacancy center (NV−) ensembles in single-crystalline diamond synthesized by either the high-pressure and high-temperature and chemical vapor deposition methods. This study specifically examined the magnetic dipole–dipole interaction (DDI) from the various electronic spin baths, which are the source of T2 decoherence. Diamond samples with NV− center concentration [NV−] comparable to those of neutral substitutional nitrogen concentration [Ns0] were used for DDI estimation. Results show that the T2 of the ensemble NV− center decreased in inverse proportion to the concentration of nitrogen-related paramagnetic defects [NPM], being the sum of [Ns0], [NV−], and [NV0], which is a neutrally charged state NV center. This inversely proportional relation between T2 and [NPM] indicates that the nitrogen-related paramagnetic defects of three kinds are the main decoherence source of the ensemble NV− center in the single-crystalline diamond. We found that the DDI coefficient of NVH− center was significantly smaller than that of Ns0, the NV0 center, or the NV− center. We ascertained the DDI coefficient of the NV− center DNV− through experimentation using a linear summation of the decoherence rates of each nitrogen-related paramagnetic defect. The obtained value of 89 μs ppm for DNV− corresponds well to the value estimated from the relation between DDI coefficient and spin multiplicity.

DOI
10.1063/5.0103332

Related papers

Dipole-dipole interaction between NV- center and nitrogen related defects

Chikara Shinei, Masuyama Yuta, Masashi Miyakawa +7 more

We investigated effect of DDI of NVH- center on T2. We controlled each paramagnetic defect concentration, except for [NVH-] being nearly same regardless of synthesis method. The controlling of defect formation was carried out by the dependence of conversion efficiency Ns0 to NV center on charge ratio of [NV-] to [NV0].3 From this controlling of [Ns0], [NV-] and [NV0], the observing obvious difference of T2 caused by [NVH-] was expected. However, no difference exists in T2 despite of [NVH-] variation as shown Fig. 1(a). This fact indicates that DDI strength of the NVH- center is significantly weaker than that of Ns0, the NV0 center, or the NV- center. Decoherence contribution of NVH- center was negligible in diamond with nitrogen concentration of a few ppm.

•Nov 16, 2023•0 citations

Dipole-dipole interaction between ensemble of NV- centers in diamond

Chikara Shinei, Masuyama Yuta, Y. MASUYAMA +8 more

Nitrogen doped diamond single crystals grown using either HPHT synthesis or CVD method were examined. After the diamond growth, electron beam irradiation and post annealing at 1000℃ for 2h were carried out to form NV-centers in the diamond crystals. For creating NV- center whose amount is comparable to that of neutral substitutional nitrogen Ns0, the total fluences of electron beam was set in the range of 1×1017 to 1×1018 e/cm-2. The 1/T2 can be expressed as summation of 1/T2{Ns0}, 1/T2{NV-} and T2{NV0}.2 By removing of the relaxation rate from Ns0 and NV0 center from 1/T2, we obtained the inverse relationship between T2{NV-} and [NV-] as shown in figure. The inverse relationship shows that DDI between NV centers is successfully detected. It is clarified that strength of DDI from NV- center: DNV- is about twice as large as those of Ns0 and NV0 center.2 It is expected that the large strength of DDI leads to shorten T2 with increasing of [NV-].

•Sep 13, 2023•0 citations

Characterization and optimization of NV centers in CVD diamond for sensing applications

Tingpeng Luo, Lukas Lindner, Julia Langer +13 more

The negatively charged nitrogen-vacancy (NV-) center in diamond is a promising spin system for quantum sensing applications. NV-ensembles are favored for an improved signal-to-noise ratio and sensitivity. The optimization of diamond with NV-ensembles often requires a high NV concentration, a long spin coherence time T2 and a stable charge state. However, these key requirements are interdependent and can be difficult to optimize: nitrogen impurities as the main decoherence source of the NV spin limits the coherence time T2, and pursuing high NV concentration can deteriorate the NV-charge-state stability. Consequently, their best achievable combination becomes an essential question for the material characterization. In this work, we systematically investigate the NV center creation and properties in chemical vapor deposition (CVD) diamond. We have grown CVD diamond series with a varying nitrogen flow over four orders of magnitude, leading to a broad range of single substitutional nitrogen (P1 center) densities from 0.2 to 20 ppm. On these series, we study P1, NV creations and NV charge states after growth, as well as their transformation under subsequent electron beam irradiation. Furthermore, for a fixed nitrogen concentration, we optimize electron-irradiation fluences with two different accelerated electron energies. We discuss a general approach to determine the optimal irradiation conditions, for which an enhanced NV concentration and an optimum of NV charge states can both be satisfied. Moreover, through irradiation and annealing treatments, we monitor the change in T2 and aim to increase the NV density without compromising T2. We achieve NV concentrations from 1 to 168 ppb with T2 from 549 to 45.5 µs respectively. This study shows a pathway to engineer properties of NV-doped CVD diamonds for improved sensitivity.

•Jun 8, 2022•0 citations

Creation of nitrogen-vacancy centers in chemical vapor deposition diamond for sensing applications

Tingpeng Luo, Lukas Lindner, J Langer +13 more

Abstract The nitrogen-vacancy (NV) center in diamond is a promising quantum system for magnetometry applications exhibiting optical readout of minute energy shifts in its spin sub-levels. Key material requirements for NV ensembles are a high NV − concentration, a long spin coherence time and a stable charge state. However, these are interdependent and can be difficult to optimize during diamond growth and subsequent NV creation. In this work, we systematically investigate the NV center formation and properties in bulk chemical vapor deposition (CVD) diamond. The nitrogen flow during growth is varied by over four orders of magnitude, resulting in a broad range of single substitutional nitrogen concentrations of 0.2–20 parts per million. For a fixed nitrogen concentration, we optimize electron-irradiation fluences with two different accelerated electron energies, and we study defect formation via optical characterizations. We discuss a general approach to determine the optimal irradiation conditions, for which an enhanced NV concentration and an optimum of NV charge states can both be satisfied. We achieve spin–spin coherence times T 2 ranging from 45.5 to 549 μ s for CVD diamonds containing 168 to 1 parts per billion NV − centers, respectively. This study shows a pathway to engineer properties of NV-doped CVD diamonds for improved sensitivity.

arXiv:2111.07981•New Journal of Physics•Feb 25, 2022•87 citations

Decoherence of nitrogen-vacancy spin ensembles in a nitrogen electron-nuclear spin bath in diamond

Huijin Park, Jung‐Hyun Lee, Sang-Wook Han +2 more

Abstract Nitrogen-vacancy (NV) centers in diamond have been developed into essential hardware units for a wide range of solid-state-based quantum technology applications. While such applications require the long spin coherence times of the NV centers, they are often limited due to decoherence. In this study, we theoretically investigate the decoherence of NV-spin ensembles induced by nitrogen impurities (P1 centers), which are one of the most dominant and inevitable magnetic field noise sources in diamond. We combined cluster correlation expansion and density functional theory to compute the Hahn-echo spin-coherence time of the NV centers for a broad range of P1 concentrations. Results indicate a clear linear dependence of T2 on P1 concentrations on a log scale with a slope of −1.06, which is in excellent agreement with previous experimental results. The interplay between the Jahn–Teller effect and the hyperfine interaction in the P1 center plays a critical role in determining the bath dynamics and the resulting NV decoherence. Our results provide a theoretical upper bound for the NV-spin T2 over a wide range of P1 densities, serving as a key reference for materials optimization and spin bath characterization to develop highly coherent NV-based devices for quantum information technology.

npj Quantum Information•Aug 12, 2022•54 citations

Quantum properties of NV centers in diamond: towards optimized industrial protocols

Léonard Desvignes, Ovidiu Brinza, Alexandre Tallaire +5 more

Because of their high sensitivity, quantum materials are extremely promising for new technologies. The main challenge lies in maintaining a sufficiently quantum coherence times for quantum computation or quantum sensing systems. NV centers in diamond which are point defects consisting of a substitutional nitrogen atom neighboring an atomic vacancy, where an electron pair can reside in a triplet state – are ideal candidates for the development of industrial-scale quantum systems. These spin states exhibit ms-long coherence times at room temperature and can be manipulated optically, hence opening interesting perspectives for sending magnetic fields with high sensitivity1.At HiQuTe Diamond, we take up the challenge of mastering the entire nitrogen-doped diamond production chain synthesized by Microwave Plasma-Assisted Chemical Vapor Deposition (MPACVD). We aim at creating affordable diamonds specially engineered to achieve long coherence times with high NV density and high doping uniformity. This quest require to overcome the impact of several external factors that contribute to electron spin decoherence. First, the chemical composition of the diamond, specifically the types and concentrations of impurities within the diamond matrix (such as substitutional nitrogen NS, NV centres, mono-vacancies and clusters, hydrogen, etc.), as well as their electrical charge states (NS⁰, NS⁺, NV⁰, NV⁻) should be carefully controlled. Thanks to extensive scientific research conducted over the past decade, combined with our own R&D efforts, we are now able to quantify these parameters using experimental techniques compatible with industrial applications (Raman and UV-Vis spectroscopy) and compare our results with key performance indicators2. Second, we study the relationship between coherence (T2*) and strain inhomogeneities in our diamond layers, which we analyse using birefringence measurements. Our findings demonstrate our capability to produce CVD diamond layers with reduced strain and extended defect and confirm that strain could be a critical limiting factor for T2*.In this poster, I will review the efforts carried out at HiQuTe Diamond to develop specific material that is well suited for quantum sensing applications.References1.Barry, J. F., Schloss, J. M., Bauch, E., Turner, M. J., Hart, C. A., Pham, L. M., & Walsworth, R. L. (2020). Sensitivity optimization for NV-diamond magnetometry. Reviews of Modern Physics, 92(1), 015004.2.Langer, J. (2022). Quantum-grade diamond for cavity-based solutions. Fraunhofer Verlag.

•Mar 19, 2025•0 citations
We investigated spin-echo coherence times T2 of negatively charged nitrogen vacancy center (NV−) ensembles in single-crystalline diamond synthesized by either the high-pressure and high-temperature and chemical vapor deposition methods. This study specifically examined the magnetic dipole–dipole interaction (DDI) from the various electronic spin baths, which are the source of T2 decoherence. Diamond samples with NV− center concentration [NV−] comparable to those of neutral substitutional nitrogen concentration [Ns0] were used for DDI estimation. Results show that the T2 of the ensemble NV− center decreased in inverse proportion to the concentration of nitrogen-related paramagnetic defects [NPM], being the sum of [Ns0], [NV−], and [NV0], which is a neutrally charged state NV center. This inversely proportional relation between T2 and [NPM] indicates that the nitrogen-related paramagnetic defects of three kinds are the main decoherence source of the ensemble NV− center in the single-crystalline diamond. We found that the DDI coefficient of NVH− center was significantly smaller than that of Ns0, the NV0 center, or the NV− center. We ascertained the DDI coefficient of the NV− center DNV− through experimentation using a linear summation of the decoherence rates of each nitrogen-related paramagnetic defect. The obtained value of 89 μs ppm for DNV− corresponds well to the value estimated from the relation between DDI coefficient and spin multiplicity.
We investigated effect of DDI of NVH- center on T2. We controlled each paramagnetic defect concentration, except for [NVH-] being nearly same regardless of synthesis method. The controlling of defect formation was carried out by the dependence of conversion efficiency Ns0 to NV center on charge ratio of [NV-] to [NV0].3 From this controlling of [Ns0], [NV-] and [NV0], the observing obvious difference of T2 caused by [NVH-] was expected. However, no difference exists in T2 despite of [NVH-] variation as shown Fig. 1(a). This fact indicates that DDI strength of the NVH- center is significantly weaker than that of Ns0, the NV0 center, or the NV- center. Decoherence contribution of NVH- center was negligible in diamond with nitrogen concentration of a few ppm.
Nitrogen doped diamond single crystals grown using either HPHT synthesis or CVD method were examined. After the diamond growth, electron beam irradiation and post annealing at 1000℃ for 2h were carried out to form NV-centers in the diamond crystals. For creating NV- center whose amount is comparable to that of neutral substitutional nitrogen Ns0, the total fluences of electron beam was set in the range of 1×1017 to 1×1018 e/cm-2. The 1/T2 can be expressed as summation of 1/T2{Ns0}, 1/T2{NV-} and T2{NV0}.2 By removing of the relaxation rate from Ns0 and NV0 center from 1/T2, we obtained the inverse relationship between T2{NV-} and [NV-] as shown in figure. The inverse relationship shows that DDI between NV centers is successfully detected. It is clarified that strength of DDI from NV- center: DNV- is about twice as large as those of Ns0 and NV0 center.2 It is expected that the large strength of DDI leads to shorten T2 with increasing of [NV-].
The negatively charged nitrogen-vacancy (NV-) center in diamond is a promising spin system for quantum sensing applications. NV-ensembles are favored for an improved signal-to-noise ratio and sensitivity. The optimization of diamond with NV-ensembles often requires a high NV concentration, a long spin coherence time T2 and a stable charge state. However, these key requirements are interdependent and can be difficult to optimize: nitrogen impurities as the main decoherence source of the NV spin limits the coherence time T2, and pursuing high NV concentration can deteriorate the NV-charge-state stability. Consequently, their best achievable combination becomes an essential question for the material characterization. In this work, we systematically investigate the NV center creation and properties in chemical vapor deposition (CVD) diamond. We have grown CVD diamond series with a varying nitrogen flow over four orders of magnitude, leading to a broad range of single substitutional nitrogen (P1 center) densities from 0.2 to 20 ppm. On these series, we study P1, NV creations and NV charge states after growth, as well as their transformation under subsequent electron beam irradiation. Furthermore, for a fixed nitrogen concentration, we optimize electron-irradiation fluences with two different accelerated electron energies. We discuss a general approach to determine the optimal irradiation conditions, for which an enhanced NV concentration and an optimum of NV charge states can both be satisfied. Moreover, through irradiation and annealing treatments, we monitor the change in T2 and aim to increase the NV density without compromising T2. We achieve NV concentrations from 1 to 168 ppb with T2 from 549 to 45.5 µs respectively. This study shows a pathway to engineer properties of NV-doped CVD diamonds for improved sensitivity.
Abstract The nitrogen-vacancy (NV) center in diamond is a promising quantum system for magnetometry applications exhibiting optical readout of minute energy shifts in its spin sub-levels. Key material requirements for NV ensembles are a high NV − concentration, a long spin coherence time and a stable charge state. However, these are interdependent and can be difficult to optimize during diamond growth and subsequent NV creation. In this work, we systematically investigate the NV center formation and properties in bulk chemical vapor deposition (CVD) diamond. The nitrogen flow during growth is varied by over four orders of magnitude, resulting in a broad range of single substitutional nitrogen concentrations of 0.2–20 parts per million. For a fixed nitrogen concentration, we optimize electron-irradiation fluences with two different accelerated electron energies, and we study defect formation via optical characterizations. We discuss a general approach to determine the optimal irradiation conditions, for which an enhanced NV concentration and an optimum of NV charge states can both be satisfied. We achieve spin–spin coherence times T 2 ranging from 45.5 to 549 μ s for CVD diamonds containing 168 to 1 parts per billion NV − centers, respectively. This study shows a pathway to engineer properties of NV-doped CVD diamonds for improved sensitivity.
Abstract Nitrogen-vacancy (NV) centers in diamond have been developed into essential hardware units for a wide range of solid-state-based quantum technology applications. While such applications require the long spin coherence times of the NV centers, they are often limited due to decoherence. In this study, we theoretically investigate the decoherence of NV-spin ensembles induced by nitrogen impurities (P1 centers), which are one of the most dominant and inevitable magnetic field noise sources in diamond. We combined cluster correlation expansion and density functional theory to compute the Hahn-echo spin-coherence time of the NV centers for a broad range of P1 concentrations. Results indicate a clear linear dependence of T2 on P1 concentrations on a log scale with a slope of −1.06, which is in excellent agreement with previous experimental results. The interplay between the Jahn–Teller effect and the hyperfine interaction in the P1 center plays a critical role in determining the bath dynamics and the resulting NV decoherence. Our results provide a theoretical upper bound for the NV-spin T2 over a wide range of P1 densities, serving as a key reference for materials optimization and spin bath characterization to develop highly coherent NV-based devices for quantum information technology.
Because of their high sensitivity, quantum materials are extremely promising for new technologies. The main challenge lies in maintaining a sufficiently quantum coherence times for quantum computation or quantum sensing systems. NV centers in diamond which are point defects consisting of a substitutional nitrogen atom neighboring an atomic vacancy, where an electron pair can reside in a triplet state – are ideal candidates for the development of industrial-scale quantum systems. These spin states exhibit ms-long coherence times at room temperature and can be manipulated optically, hence opening interesting perspectives for sending magnetic fields with high sensitivity1.At HiQuTe Diamond, we take up the challenge of mastering the entire nitrogen-doped diamond production chain synthesized by Microwave Plasma-Assisted Chemical Vapor Deposition (MPACVD). We aim at creating affordable diamonds specially engineered to achieve long coherence times with high NV density and high doping uniformity. This quest require to overcome the impact of several external factors that contribute to electron spin decoherence. First, the chemical composition of the diamond, specifically the types and concentrations of impurities within the diamond matrix (such as substitutional nitrogen NS, NV centres, mono-vacancies and clusters, hydrogen, etc.), as well as their electrical charge states (NS⁰, NS⁺, NV⁰, NV⁻) should be carefully controlled. Thanks to extensive scientific research conducted over the past decade, combined with our own R&D efforts, we are now able to quantify these parameters using experimental techniques compatible with industrial applications (Raman and UV-Vis spectroscopy) and compare our results with key performance indicators2. Second, we study the relationship between coherence (T2*) and strain inhomogeneities in our diamond layers, which we analyse using birefringence measurements. Our findings demonstrate our capability to produce CVD diamond layers with reduced strain and extended defect and confirm that strain could be a critical limiting factor for T2*.In this poster, I will review the efforts carried out at HiQuTe Diamond to develop specific material that is well suited for quantum sensing applications.References1.Barry, J. F., Schloss, J. M., Bauch, E., Turner, M. J., Hart, C. A., Pham, L. M., & Walsworth, R. L. (2020). Sensitivity optimization for NV-diamond magnetometry. Reviews of Modern Physics, 92(1), 015004.2.Langer, J. (2022). Quantum-grade diamond for cavity-based solutions. Fraunhofer Verlag.