Low-Power Optical Bistability in Cadmium Sulfide Platelets

M. Dagenais, Wayne F. Sharfin, Herbert G. Winful

Published Jun 18, 1984• 2 citations
OpenAlex

Abstract

We report the observation of transverse and whole-beam optical bistability in thin uncoated cadmium sulfide platelets at milliwatt power levels when a laser is tuned to the vicinity of a bound exciton resonance. The characteristics of both processes are quite different and are described separately.

Related papers

Cavityless optical bistability due to light-induced absorption in cadmium sulfide

M. Dagenais, Wayne F. Sharfin

Cavityless, whole-beam optical bistability in thin, uncoated cadmium sulfide platelets is observed at milliwatt power levels when a cw laser is tuned near a sharp extrinsic excitonic resonance in cadmium sulfide (the I2 bound exciton). Very large contrast ratios between the on and off states are measured. The detuning and temperature dependence of the bistability results are reported. Preliminary transient measurements are also discussed.

Applied Physics Letters•Aug 1, 1984•70 citations

Giant nonlinearities and low power optical bistability in cadmium sulphide platelets

M. Dagenais

Abstract Both whole-beam and transverse continuous wave optical bistability are observed at milliwatt power levels near the band gap in thin uncoated cadmium sulphide platelets. The whole-beam bistability is free from cavities and requires an absorption coefficient that increases with intensity.

Philosophical Transactions of the Royal Society of London Series A Mathematical and Physical Sciences•Dec 18, 1984•1 citation

Low power transverse optical bistability near bound excitons in cadmium sulfide

M. Dagenais, Herbert G. Winful

We report the observation of cw transverse optical bistability without power hysteresis at 1-mW power levels in uncoated cadmium sulfide platelets. Optically induced refractive index changes as large as 0.15 are deduced from measurements of the transverse spatial ring profile.

Applied Physics Letters•Mar 15, 1984•33 citations

Low-power saturation of bound excitons and observation of optical bistability

M. Dagenais, Herbert G. Winful

Very large nonlinearities are observed in the vicinity of a bound exciton resonance in cadmium sulfide. Power levels of the order of 8 μW are sufficient for saturating the bound exciton resonance in a tight focusing geometry. In a more loosely focused geometry, power levels of the order of 250 μW are sufficient for saturating the bound exciton resonance and for observing optical bistability. Transverse effects are found to play a very important role. For all our measurements, no thermal contributions to the nonlinearity were observed. Since thermal effects are not playing a role and since the studied bound excitons decay radiatively in 500 psec, we infer subnanosecond switchoff and cycling times.

Conference on Lasers and Electro-Optics•Jan 1, 1983•1 citation

Low Power Optical Bistability near Bound Excitons in Cadmium Sulfide

M. Dagenais, Herbert G. Winful

Springer eBooks•Jan 1, 1984•3 citations

Low Power Optical Bistability Near Bound Excitons in Cadmium Sulfide

M. Dagenais, H. G. Winful

The I2 bound exciton in cadmium sulfide has a giant oscillator strength of 6. It decays mostly radiatively in 500 psec. Such a large oscillator strength leads to a very large transition dipole moment and to very large nonlinear effects off-resonance. At 2K, this sytem saturates like an inhomogeneously broadened system for intensities up to 30 times the saturation intensity. The transition linewidth is 7.5 GHz. In a tight focusing geometry, only 3.6 μW is required to see the onset of saturation. This corresponds to a measured saturation intensity of about 60 W/cm2. The linear absorption coefficient right at the resonance peak was measured to be 3.2 x 103 cm-1. At higher temperatures, the transition linewidth broadens and the line becomes more and more homogeneously broadened because of phonon interaction. At intensities above 50 times the saturation intensity, the absorption coefficient stops decreasing and then starts increasing. At these high intensities, thermal effects appear to play a significant role in shifting the free and bound exciton resonances toward lower energies. At intensities less than 20 times the saturation intensity, thermal effects are believed to be insignificant in our saturation measurements.

Topical Meeting on Optical Bistability (OB)•Jan 1, 1983•0 citations
Very large nonlinearities are observed in the vicinity of a bound exciton resonance in cadmium sulfide. Power levels of the order of 8 μW are sufficient for saturating the bound exciton resonance in a tight focusing geometry. In a more loosely focused geometry, power levels of the order of 250 μW are sufficient for saturating the bound exciton resonance and for observing optical bistability. Transverse effects are found to play a very important role. For all our measurements, no thermal contributions to the nonlinearity were observed. Since thermal effects are not playing a role and since the studied bound excitons decay radiatively in 500 psec, we infer subnanosecond switchoff and cycling times.
The I2 bound exciton in cadmium sulfide has a giant oscillator strength of 6. It decays mostly radiatively in 500 psec. Such a large oscillator strength leads to a very large transition dipole moment and to very large nonlinear effects off-resonance. At 2K, this sytem saturates like an inhomogeneously broadened system for intensities up to 30 times the saturation intensity. The transition linewidth is 7.5 GHz. In a tight focusing geometry, only 3.6 μW is required to see the onset of saturation. This corresponds to a measured saturation intensity of about 60 W/cm2. The linear absorption coefficient right at the resonance peak was measured to be 3.2 x 103 cm-1. At higher temperatures, the transition linewidth broadens and the line becomes more and more homogeneously broadened because of phonon interaction. At intensities above 50 times the saturation intensity, the absorption coefficient stops decreasing and then starts increasing. At these high intensities, thermal effects appear to play a significant role in shifting the free and bound exciton resonances toward lower energies. At intensities less than 20 times the saturation intensity, thermal effects are believed to be insignificant in our saturation measurements.