Physical Review B

Effects of magnetic field orientation on optical decoherence in Er 3 + : Y 2 SiO 5

Thomas Böttger, Charles W. Thiel, R. L. Cone, Yazhou Sun

Published Mar 10, 2009• 181 citations
Publisher

Abstract

The influence of the anisotropic Zeeman effect on optical decoherence was studied for the $1.54\text{ }\ensuremath{\mu}\text{m}$ telecom transition in ${\text{Er}}^{3+}:{\text{Y}}_{2}{\text{SiO}}_{5}$ using photon echo spectroscopy as a function of applied magnetic field orientation and strength. The decoherence strongly correlates with the Zeeman energy splittings described by the ground- and excited-state $g$ factor variations for all inequivalent ${\text{Er}}^{3+}$ sites, with the observed decoherence times arising from the combined effects of the magnetic dipole-dipole coupling strength and the ground- and excited-state spin-flip rates, along with the natural lifetime of the upper level. The decoherence time was maximized along a preferred magnetic field orientation that minimized the effects of spectral diffusion and that enabled the measurement of an exceptionally narrow optical resonance in a solid---demonstrating a homogeneous linewidth as narrow as 73 Hz.

DOI
10.1103/physrevb.79.115104

Related papers

Optical decoherence, spectroscopy, and magnetic g tensors for the 1.5-µm I 15 / 2 4 − I 13 / 2 4 transitions of E r 3 + dopants at the C 2 -symmetry site in Y 2 O 3

Thomas Böttger, Todd L. Harris, G. D. Reinemer +2 more

Erbium-doped solids are a promising platform for quantum technology due to the $\mathrm{E}{\mathrm{r}}^{3+}$ 1.5-\textmu{}m optical transition in the telecom C band that can offer long coherence times. To characterize the intrinsic ${\mathrm{C}}_{2}$ site of $\mathrm{E}{\mathrm{r}}^{3+}$ in ${\mathrm{Y}}_{2}{\mathrm{O}}_{3}$ for quantum information and photonic signal-processing applications, absorption and site-selective fluorescence spectroscopy were used to assign the $\mathrm{E}{\mathrm{r}}^{3+}\phantom{\rule{4pt}{0ex}}^{4}I_{15/2}$$\ensuremath{\leftrightarrow}$$^{4}I_{13/2}$ transitions. The lowest-to-lowest transition occurs at 1535.608 nm and laser absorption determined an inhomogeneous linewidth of 780 MHz in a 0.005%-doped crystal at 3.4 K. Time-resolved fluorescence established an upper limit for the excited-state lifetime of 8.5 ms. Angular-dependent Zeeman absorption was used to determine ground- and excited-state $g$ tensors. The ${\mathrm{C}}_{2}$-site $g$ tensor components for the ground state are ${g}_{x}=1.60$, ${g}_{y}=4.71$, and ${g}_{z}=11.93$ with a tipping angle of \ensuremath{\alpha} = $2.{06}^{\ensuremath{\circ}}$, whereas for the excited state the components are ${g}_{x}=1.08$, ${g}_{y}=4.36$, and ${g}_{z}=10.07$ with a tipping angle of \ensuremath{\alpha} = $\ensuremath{-}11.{7}^{\ensuremath{\circ}}$. Optical decoherence can be suppressed by the application of a magnetic field parallel to $\ensuremath{\langle}111\ensuremath{\rangle}$ crystal axes where all ${\mathrm{C}}_{2}$ sites become nearly magnetically equivalent with large $g$ values so that spin flips of neighboring $\mathrm{E}{\mathrm{r}}^{3+}$ ions can be simultaneously suppressed. Using this magnetic field direction, two-pulse photon echoes gave a homogeneous linewidth of 5 kHz for an applied magnetic field of 0.5 T, narrowing and saturating at 2.5 kHz at 3.5 T. Decoherence over intermediate magnetic fields was described by spectral diffusion due to $\mathrm{E}{\mathrm{r}}^{3+}\text{\ensuremath{-}}\mathrm{E}{\mathrm{r}}^{3+}$ magnetic dipole interactions driven by the direct phonon process. With $\mathrm{E}{\mathrm{r}}^{3+}$:${\mathrm{Y}}_{2}{\mathrm{O}}_{3}$ absorption at a convenient telecom laser wavelength and the ability to fabricate waveguides, our study suggests that this is a promising material system for quantum information and spectral hole-burning signal-processing applications.

Physical review. B./Physical review. B•Jul 17, 2024•8 citations

Magnetic g tensors for the I 15 ∕ 2 4 and I 13 ∕ 2 4 states of Er 3 + : Y 2 Si O 5

Yongchen Sun, Thomas Böttger, Charles W. Thiel +1 more

We present the complete Zeeman $g$ tensors for the lowest-energy $^{4}\mathrm{I}_{15∕2}$ and $^{4}\mathrm{I}_{13∕2}$ states of ${\mathrm{Er}}^{3+}$ doped into ${\mathrm{Y}}_{2}\mathrm{Si}{\mathrm{O}}_{5}$ for both crystallographic sites deduced from orientation-dependent optical Zeeman spectroscopy over three orthogonal crystal planes. From these data, principal axes of the $g$ tensors were determined for each crystallographic site. Along axes with maximum values, the effective $g$ factors are 14.65 (site 1) and 15.46 (site 2) for the ground state, and 12.97 (site 1) and 13.77 (site 2) for the excited state. To minimize optical decoherence and spectral diffusion in device applications and high resolution spectroscopy, special directions for applying an external magnetic field have been found for each site, for which the ground- and excited-state $g$ factors are equal. Among those directions, choices are presented that also maximize the ground-state splittings for all four magnetically inequivalent sites, thus optimizing the prospects for freezing out electron spin fluctuations and reducing decoherence and spectral diffusion significantly.

Physical Review B•Feb 29, 2008•95 citations

Optical decoherence studies of yttrium oxyorthosilicate Y 2 SiO 5 codoped with Er 3 + and Eu 3 + for optical signal processing and quantum information applications at 1.5 microns

Charles W. Thiel, William Randall Babbitt, R. L. Cone

We report detailed studies of the optical decoherence and spectroscopic properties of the 1536-nm optical transition of the bandwidth-engineered material 0.02$%$Er:1$%$Eu:Y${}_{2}$SiO${}_{5}$. This work is motivated by the need for comprehensive understanding of new resonant optical materials for spatial-spectral holography and quantum information applications. The dependence of optical decoherence on excitation frequency, applied magnetic field strength and orientation, crystal temperature, measurement time scale, and optical excitation density was studied using stimulated photon echo spectroscopy and time-resolved spectral hole-burning techniques. The effects of weak disorder generated by the introduction of Eu${}^{3+}$ ions into the lattice was probed by comparing measurements across the static disorder-induced distribution of transition frequencies as well as by comparing with measurements on 0.02$%$Er:Y${}_{2}$SiO${}_{5}$. The results reveal that the coherence properties of Er:Y${}_{2}$SiO${}_{5}$ are preserved in the disordered system; moreover, the increased inhomogeneity produced by the disorder acts to suppress optical decoherence by inhibiting the electronic spin diffusion process, improving material properties for low magnetic field strengths and at increased temperatures desirable for practical applications.

Physical Review B•May 11, 2012•39 citations

Optical decoherence and spectral diffusion at 1.5 μ m in Er 3 + : Y 2 SiO 5 versus magnetic field, temperature, and Er 3 + concentration

Thomas Böttger, Charles W. Thiel, Yiwen Sun +1 more

The mechanisms and effects of spectral diffusion for optical transitions of paramagnetic ions have been explored using the inhomogeneously broadened 1536 nm $^{4}\mathrm{I}_{15∕2}\ensuremath{\rightarrow}^{4}\mathrm{I}_{13∕2}$ transition in ${\mathrm{Er}}^{3+}:{\mathrm{Y}}_{2}{\mathrm{SiO}}_{5}$. Using photon echo spectroscopy, spectral diffusion was measured by observing the evolution of the effective coherence lifetimes over time scales from $1\phantom{\rule{0.3em}{0ex}}\ensuremath{\mu}\mathrm{s}$ to 20 ms for magnetic-field strengths from 0.3 to 6.0 T, temperatures from 1.6 to 6.5 K, and nominal ${\mathrm{Er}}^{3+}$ concentrations of 0.0015%, 0.005%, and 0.02%. To understand the effect of spectral diffusion on material decoherence for different environmental conditions and material compositions, data and models were compared to identify spectral diffusion mechanisms and microscopic spin dynamics. Observations were successfully modeled by ${\mathrm{Er}}^{3+}\ensuremath{-}{\mathrm{Er}}^{3+}$ magnetic dipole interactions and ${\mathrm{Er}}^{3+}$ electron spin flips driven by the one-phonon direct process. At temperatures of 4.2 K and higher, spectral diffusion due to $^{89}\mathrm{Y}$ nuclear spin flips was also observed. The success in describing our extensive experimental results using simple models provides an important capability for exploring larger parameter spaces, accelerating the design and optimization of materials for spatial-spectral holography, and spectral hole-burning devices. The broad insight into spectral diffusion mechanisms and dynamics is applicable to other paramagnetic materials, such as those containing ${\mathrm{Yb}}^{3+}$ or ${\mathrm{Nd}}^{3+}$.

Physical Review B•Feb 1, 2006•217 citations

Optical spectroscopy, magnetic g tensors, and decoherence studies of magnetic dipole transitions of E r 3 + at C 3 i -symmetry lattice sites in Y 2 O 3 at 1.5 µm

Thomas Böttger, G. D. Reinemer, Charles W. Thiel +1 more

When introduced as dopants into ${\mathrm{Y}}_{2}{\mathrm{O}}_{3}$, $\mathrm{E}{\mathrm{r}}^{3+}$ ions replace ${\mathrm{Y}}^{3+}$ ions at two crystallographic sites of ${\mathrm{C}}_{2}$ and ${\mathrm{C}}_{3\mathrm{i}}$ point symmetries. The ${\mathrm{C}}_{3\mathrm{i}}$ site is particularly interesting, given that the inversion symmetry prohibits static electric-dipole moments and electric-dipole transitions, resulting in 1.5 \textmu{}m optical transitions characterized by purely magnetic-dipole properties. Employing $\mathrm{E}{\mathrm{r}}^{3+}\phantom{\rule{4pt}{0ex}}^{4}I_{15/2}\ensuremath{\leftrightarrow}^{4}I_{13/2}$ transitions, we examined the inherent ${\mathrm{C}}_{3\mathrm{i}}$ site of $\mathrm{E}{\mathrm{r}}^{3+}$ in ${\mathrm{Y}}_{2}{\mathrm{O}}_{3}$ for its potential in quantum information science and spectral hole burning applications. Our approach involved absorption and site-selective fluorescence spectroscopy to discern $\mathrm{E}{\mathrm{r}}^{3+}$ energy levels and revealed an excited-state lifetime of 14.6 ms. High-resolution laser spectroscopy at 3.7 K indicated an inhomogeneous linewidth of 1.3 GHz in our sample. Orientation-dependent Zeeman laser absorption spectroscopy facilitated the determination of the full $g$ tensors for both the ground and excited states, confirming the ${\mathrm{C}}_{3\mathrm{i}}$ site assignment. Furthermore, it identified a suitable magnetic field direction for mitigating decoherence, a finding corroborated through two-pulse photon echo spectroscopy. Our study presents photon echo coherent transient measurements related to magnetic-dipole-allowed rare-earth ion transitions at the ${\mathrm{C}}_{3\mathrm{i}}$ site. The observed decoherence, attributed to spectral diffusion arising from $\mathrm{E}{\mathrm{r}}^{3+}\text{\ensuremath{-}}\mathrm{E}{\mathrm{r}}^{3+}$ magnetic-dipole interactions, underscores the complex spin dynamics at play in systems with multiple inequivalent dopant sites. Coupled with the practicality of telecom laser wavelengths, our investigation highlights the promise of magnetic-dipole transitions in advancing quantum information science and spectral hole burning applications.

Physical review. B./Physical review. B•Jan 7, 2025•3 citations

Spin Dynamics of Single Er 3+ Ions in a Silicon Nanophotonic Cavity

Songtao Chen, Mouktik Raha, Christopher M. Phenicie +2 more

Magnetic field orientation and strength dependent spin dynamics is studied for the 1.536 $\mu \mathrm{m}$ telecom transitions of single Er3+ ions in Y 2 SiO 5 . Long spin $T_{1}=2$ seconds is measured from ground state Zeeman spin levels. © 2019 The Author(s)

Conference on Lasers and Electro-Optics•May 5, 2019•0 citations
The influence of the anisotropic Zeeman effect on optical decoherence was studied for the 1.54 \ensuremathμm1.54\text{ }\ensuremath{\mu}\text{m}1.54 \ensuremathμm telecom transition in Er3+:Y2SiO5{\text{Er}}^{3+}:{\text{Y}}_{2}{\text{SiO}}_{5}Er3+:Y2​SiO5​ using photon echo spectroscopy as a function of applied magnetic field orientation and strength. The decoherence strongly correlates with the Zeeman energy splittings described by the ground- and excited-state ggg factor variations for all inequivalent Er3+{\text{Er}}^{3+}Er3+ sites, with the observed decoherence times arising from the combined effects of the magnetic dipole-dipole coupling strength and the ground- and excited-state spin-flip rates, along with the natural lifetime of the upper level. The decoherence time was maximized along a preferred magnetic field orientation that minimized the effects of spectral diffusion and that enabled the measurement of an exceptionally narrow optical resonance in a solid---demonstrating a homogeneous linewidth as narrow as 73 Hz.
Erbium-doped solids are a promising platform for quantum technology due to the Er3+\mathrm{E}{\mathrm{r}}^{3+}Er3+ 1.5-\textmu{}m optical transition in the telecom C band that can offer long coherence times. To characterize the intrinsic C2{\mathrm{C}}_{2}C2​ site of Er3+\mathrm{E}{\mathrm{r}}^{3+}Er3+ in Y2O3{\mathrm{Y}}_{2}{\mathrm{O}}_{3}Y2​O3​ for quantum information and photonic signal-processing applications, absorption and site-selective fluorescence spectroscopy were used to assign the Er3+4I15/2\mathrm{E}{\mathrm{r}}^{3+}\phantom{\rule{4pt}{0ex}}^{4}I_{15/2}Er3+4I15/2​$\ensuremath{\leftrightarrow}$4I13/2^{4}I_{13/2}4I13/2​ transitions. The lowest-to-lowest transition occurs at 1535.608 nm and laser absorption determined an inhomogeneous linewidth of 780 MHz in a 0.005%-doped crystal at 3.4 K. Time-resolved fluorescence established an upper limit for the excited-state lifetime of 8.5 ms. Angular-dependent Zeeman absorption was used to determine ground- and excited-state ggg tensors. The C2{\mathrm{C}}_{2}C2​-site ggg tensor components for the ground state are gx=1.60{g}_{x}=1.60gx​=1.60, gy=4.71{g}_{y}=4.71gy​=4.71, and gz=11.93{g}_{z}=11.93gz​=11.93 with a tipping angle of \ensuremath{\alpha} = $2.{06}^{\ensuremath{\circ}}$, whereas for the excited state the components are gx=1.08{g}_{x}=1.08gx​=1.08, gy=4.36{g}_{y}=4.36gy​=4.36, and gz=10.07{g}_{z}=10.07gz​=10.07 with a tipping angle of \ensuremath{\alpha} = $\ensuremath{-}11.{7}^{\ensuremath{\circ}}$. Optical decoherence can be suppressed by the application of a magnetic field parallel to $\ensuremath{\langle}111\ensuremath{\rangle}$ crystal axes where all C2{\mathrm{C}}_{2}C2​ sites become nearly magnetically equivalent with large ggg values so that spin flips of neighboring Er3+\mathrm{E}{\mathrm{r}}^{3+}Er3+ ions can be simultaneously suppressed. Using this magnetic field direction, two-pulse photon echoes gave a homogeneous linewidth of 5 kHz for an applied magnetic field of 0.5 T, narrowing and saturating at 2.5 kHz at 3.5 T. Decoherence over intermediate magnetic fields was described by spectral diffusion due to $\mathrm{E}{\mathrm{r}}^{3+}\text{\ensuremath{-}}\mathrm{E}{\mathrm{r}}^{3+}$ magnetic dipole interactions driven by the direct phonon process. With Er3+\mathrm{E}{\mathrm{r}}^{3+}Er3+:Y2O3{\mathrm{Y}}_{2}{\mathrm{O}}_{3}Y2​O3​ absorption at a convenient telecom laser wavelength and the ability to fabricate waveguides, our study suggests that this is a promising material system for quantum information and spectral hole-burning signal-processing applications.
We present the complete Zeeman ggg tensors for the lowest-energy 4I15∕2^{4}\mathrm{I}_{15∕2}4I15∕2​ and 4I13∕2^{4}\mathrm{I}_{13∕2}4I13∕2​ states of Er3+{\mathrm{Er}}^{3+}Er3+ doped into Y2SiO5{\mathrm{Y}}_{2}\mathrm{Si}{\mathrm{O}}_{5}Y2​SiO5​ for both crystallographic sites deduced from orientation-dependent optical Zeeman spectroscopy over three orthogonal crystal planes. From these data, principal axes of the ggg tensors were determined for each crystallographic site. Along axes with maximum values, the effective ggg factors are 14.65 (site 1) and 15.46 (site 2) for the ground state, and 12.97 (site 1) and 13.77 (site 2) for the excited state. To minimize optical decoherence and spectral diffusion in device applications and high resolution spectroscopy, special directions for applying an external magnetic field have been found for each site, for which the ground- and excited-state ggg factors are equal. Among those directions, choices are presented that also maximize the ground-state splittings for all four magnetically inequivalent sites, thus optimizing the prospects for freezing out electron spin fluctuations and reducing decoherence and spectral diffusion significantly.
We report detailed studies of the optical decoherence and spectroscopic properties of the 1536-nm optical transition of the bandwidth-engineered material 0.02%Er:1%Eu:Y2{}_{2}2​SiO5{}_{5}5​. This work is motivated by the need for comprehensive understanding of new resonant optical materials for spatial-spectral holography and quantum information applications. The dependence of optical decoherence on excitation frequency, applied magnetic field strength and orientation, crystal temperature, measurement time scale, and optical excitation density was studied using stimulated photon echo spectroscopy and time-resolved spectral hole-burning techniques. The effects of weak disorder generated by the introduction of Eu3+{}^{3+}3+ ions into the lattice was probed by comparing measurements across the static disorder-induced distribution of transition frequencies as well as by comparing with measurements on 0.02%Er:Y2{}_{2}2​SiO5{}_{5}5​. The results reveal that the coherence properties of Er:Y2{}_{2}2​SiO5{}_{5}5​ are preserved in the disordered system; moreover, the increased inhomogeneity produced by the disorder acts to suppress optical decoherence by inhibiting the electronic spin diffusion process, improving material properties for low magnetic field strengths and at increased temperatures desirable for practical applications.
The mechanisms and effects of spectral diffusion for optical transitions of paramagnetic ions have been explored using the inhomogeneously broadened 1536 nm $^{4}\mathrm{I}_{15∕2}\ensuremath{\rightarrow}^{4}\mathrm{I}_{13∕2}$ transition in Er3+:Y2SiO5{\mathrm{Er}}^{3+}:{\mathrm{Y}}_{2}{\mathrm{SiO}}_{5}Er3+:Y2​SiO5​. Using photon echo spectroscopy, spectral diffusion was measured by observing the evolution of the effective coherence lifetimes over time scales from $1\phantom{\rule{0.3em}{0ex}}\ensuremath{\mu}\mathrm{s}$ to 20 ms for magnetic-field strengths from 0.3 to 6.0 T, temperatures from 1.6 to 6.5 K, and nominal Er3+{\mathrm{Er}}^{3+}Er3+ concentrations of 0.0015%, 0.005%, and 0.02%. To understand the effect of spectral diffusion on material decoherence for different environmental conditions and material compositions, data and models were compared to identify spectral diffusion mechanisms and microscopic spin dynamics. Observations were successfully modeled by ${\mathrm{Er}}^{3+}\ensuremath{-}{\mathrm{Er}}^{3+}$ magnetic dipole interactions and Er3+{\mathrm{Er}}^{3+}Er3+ electron spin flips driven by the one-phonon direct process. At temperatures of 4.2 K and higher, spectral diffusion due to 89Y^{89}\mathrm{Y}89Y nuclear spin flips was also observed. The success in describing our extensive experimental results using simple models provides an important capability for exploring larger parameter spaces, accelerating the design and optimization of materials for spatial-spectral holography, and spectral hole-burning devices. The broad insight into spectral diffusion mechanisms and dynamics is applicable to other paramagnetic materials, such as those containing Yb3+{\mathrm{Yb}}^{3+}Yb3+ or Nd3+{\mathrm{Nd}}^{3+}Nd3+.
When introduced as dopants into Y2O3{\mathrm{Y}}_{2}{\mathrm{O}}_{3}Y2​O3​, Er3+\mathrm{E}{\mathrm{r}}^{3+}Er3+ ions replace Y3+{\mathrm{Y}}^{3+}Y3+ ions at two crystallographic sites of C2{\mathrm{C}}_{2}C2​ and C3i{\mathrm{C}}_{3\mathrm{i}}C3i​ point symmetries. The C3i{\mathrm{C}}_{3\mathrm{i}}C3i​ site is particularly interesting, given that the inversion symmetry prohibits static electric-dipole moments and electric-dipole transitions, resulting in 1.5 \textmu{}m optical transitions characterized by purely magnetic-dipole properties. Employing $\mathrm{E}{\mathrm{r}}^{3+}\phantom{\rule{4pt}{0ex}}^{4}I_{15/2}\ensuremath{\leftrightarrow}^{4}I_{13/2}$ transitions, we examined the inherent C3i{\mathrm{C}}_{3\mathrm{i}}C3i​ site of Er3+\mathrm{E}{\mathrm{r}}^{3+}Er3+ in Y2O3{\mathrm{Y}}_{2}{\mathrm{O}}_{3}Y2​O3​ for its potential in quantum information science and spectral hole burning applications. Our approach involved absorption and site-selective fluorescence spectroscopy to discern Er3+\mathrm{E}{\mathrm{r}}^{3+}Er3+ energy levels and revealed an excited-state lifetime of 14.6 ms. High-resolution laser spectroscopy at 3.7 K indicated an inhomogeneous linewidth of 1.3 GHz in our sample. Orientation-dependent Zeeman laser absorption spectroscopy facilitated the determination of the full ggg tensors for both the ground and excited states, confirming the C3i{\mathrm{C}}_{3\mathrm{i}}C3i​ site assignment. Furthermore, it identified a suitable magnetic field direction for mitigating decoherence, a finding corroborated through two-pulse photon echo spectroscopy. Our study presents photon echo coherent transient measurements related to magnetic-dipole-allowed rare-earth ion transitions at the C3i{\mathrm{C}}_{3\mathrm{i}}C3i​ site. The observed decoherence, attributed to spectral diffusion arising from $\mathrm{E}{\mathrm{r}}^{3+}\text{\ensuremath{-}}\mathrm{E}{\mathrm{r}}^{3+}$ magnetic-dipole interactions, underscores the complex spin dynamics at play in systems with multiple inequivalent dopant sites. Coupled with the practicality of telecom laser wavelengths, our investigation highlights the promise of magnetic-dipole transitions in advancing quantum information science and spectral hole burning applications.
Magnetic field orientation and strength dependent spin dynamics is studied for the 1.536 μm\mu \mathrm{m}μm telecom transitions of single Er3+ ions in Y 2 SiO 5 . Long spin T1=2T_{1}=2T1​=2 seconds is measured from ground state Zeeman spin levels. © 2019 The Author(s)