arXiv:2610.16468
Deterministic positioning accuracy of B centers in hBN by electron irradiation
A. Núñez Marcos, C. Arnold, J. Barjon, S. Buil, J. -P. Hermier, A. Delteil
Abstract
Hexagonal boron nitride (hBN) is a promising material platform for quantum technologies, enabling both the realization of nanophotonic devices and the hosting of point defects that act as high-quality single-photon emitters (SPEs). Among these defects, B centers, which reproducibly emit at 436 nm, can be generated individually at predefined positions using electron beam irradiation, a crucial capability for top-down quantum photonics. Yet, the spatial accuracy of emitter creation strongly conditions the potential applications. Here, we generate arrays of individual B centers in a scanning electron microscope (SEM) with in-situ cathodoluminescence (CL) monitoring. We characterize the sources of random deviations from the target positions to identify the limitations to their deterministic positioning. In particular, we measure the distance between the electron beam and the emitter at the moment the emitter is created based on CL mapping. This approach provides a direct estimation of the spatial extent of the beam-emitter interaction. We find this contribution to be the main constraint to the emitter fabrication accuracy, yielding a standard deviation of 27 nm. Additional contributions, primarily from the finite density of UV-emitting carbon dimer precursors, increase the overall positional standard deviation to 40 nm. Our results highlight the possible improvements to the B center creation technique to reach sub-10 nm accuracy.
AI Summary
The paper investigates the in-plane positioning accuracy of electron-beam-created B centers in hBN, single-photon emitters at 436 nm, and separates the contributions limiting placement. Arrays are fabricated in a scanning electron microscope using 3 kV irradiation and real-time cathodoluminescence (CL) feedback: irradiation at each target stops when a B center appears. Photoluminescence localization of 75 emitters across six arrays gives a per-coordinate positional standard deviation of $39.9\pm2.8$ nm relative to fitted target grids. The grid fitting removes systematic geometric distortions, so this measures stochastic relative placement rather than absolute registration. Activation events captured during CL scanning provide a separate measurement: fitting truncated emission spots locates both the emitter and the beam at activation. Across 29 events, their separation follows a Rayleigh distribution with scale $26.8\pm2.5$ nm, substantially narrower than the approximately 110 nm CL excitation width. An error budget combines beam positioning ($18\pm1$ nm), optical localization ($8\pm4$ nm), the measured activation width, and a precursor-density contribution estimated as $22.6\pm3.7$ nm. Their quadrature sum is 40.2 nm. The density contribution uses a Poisson-distributed-precursor model with approximately Gaussian placement statistics. Electron-transport simulations predict narrower energy deposition than measured; imperfect focusing and uncertain low-voltage simulation accuracy are cited as explanations. Sub-10 nm placement is proposed, not demonstrated, through thinner crystals, higher carbon-dimer precursor density, and improved beam control. The study addresses lateral accuracy; vertical placement is bounded by the crystal interfaces.
Error found: The reported surface precursor density gives a density-related positional contribution of 9.03 nm under the paper's formula, rather than 22.6 nm, changing the calculated total spread from 40.2 nm to 34.46 nm. The reported volume precursor density and 86 nm thickness imply a surface density of 3.096 × 10^10 cm⁻², approximately 2π smaller than the printed value; this corrected density does reproduce the reported 22.6 nm contribution. The truncated-Gaussian fitting equation is printed with a positive exponent instead of the negative exponent required for a localized spot.
Written by gpt-6.1-sol from the paper's full text. Automated: it can be wrong.