arXiv:2610.01183
Additive solid immersion lenses for enhanced collection efficiency of shallow NV centers by pulsed laser deposition and structurization of high-k amorphous oxides
Michael S. Bar, Nicole Raatz, Max Kneiss, Andreas Koenig, Marius Grundmann, Holger von Wenckstern
Abstract
The negatively charged nitrogen-vacancy ($\mathrm{NV}^-$) defect in diamond can be used for quantum information processing via the readout of the radiative decay of the excited state into the ground state. The large refractive index mismatch of diamond and air causes low photon extraction efficiency due to total internal reflection losses. Here, we investigate the photon extraction numerically and report additive solid immersion lenses (SILs) consisting of the high-k dielectric yttria-stabilized-zirconia (YSZ) for surface modification and enhanced light extraction of shallow implanted nitrogen-vacancy centers. We demonstrate an average increase of 63% in saturation intensity using a scalable bottum up room temperature pulsed laser deposition and photolithography structurization process. The average necessary laser intensity for saturation is reduced by 33% by the SILs.
AI Summary
Shallow NV centers cannot readily use solid immersion lenses (SILs) carved into diamond because they lie only tens of nanometers below the surface. This paper investigates additive yttria-stabilized-zirconia (YSZ) SILs for improving photon extraction without machining the diamond. Monte Carlo geometric-optics simulations examine refractive-index matching, lateral misalignment and departures from hemispherical geometry. Ideal lenses with refractive index near $2.1$ give approximately sixfold extraction enhancement; larger lenses tolerate greater absolute placement errors. Room-temperature pulsed laser deposition through patterned photoresist, with oblique deposition and sample rotation, produces curved lens arrays. The deposited YSZ has refractive index $n=2.17$ at 632 nm and fluorescence comparable to the diamond reference under the tested excitation conditions. Confocal measurements compare shallow implanted NV centers beneath SILs, beneath planar YSZ and on untreated diamond. Mean background-corrected saturation counts increase from 96 kc/s on bare diamond to 160 kc/s beneath SILs, a 63% enhancement; planar YSZ gives 98 kc/s. Mean saturation power decreases from 3.6 to 2.5 mW, reported as a 33% reduction. Simulations using measured lens topography reproduce the observed offset dependence reasonably for NV centers 1–3 $\mu$m from lens centers. The measurements pool single NVs and pairs, with and without sulfur co-doping, contributing to variability. Centrally located NVs have limited statistics. Fabrication leaves peripheral “fencing” of uncertain optical effect. The model omits wave optics, NV dipole-emission anisotropy, multiple internal reflections and collection numerical aperture. The mechanism behind reduced saturation power remains unresolved.
Central claim may not hold: The reported saturation-count means imply a 66.7% increase over bare diamond, while the claimed 63% matches the planar-YSZ reference instead. The reported excitation reduction concerns nominal laser power, whereas the abstract calls it an intensity reduction without establishing local excitation intensity. Pooling emitters with different doping and emitter multiplicity without reporting their distribution across surface conditions leaves the causal attribution of the average enhancement to the SILs conditional.
Written by gpt-6.1-sol from the paper's full text. Automated: it can be wrong.