The elucidation of the mechanism of SnV− formation in diamond is especially important as the SnV− color center has the potential to be a superior single-photon emitter when compared to the NV and to other Group IV impurity-vacancy color centers in diamond. The typical formation of SnV involves placing Sn in diamond by ion implantation, but the formation of a charged SnV species requires an additional complication. This complication is related to the energy cost associated with electronic transitions within the host diamond. Effectively, producing the SnV− charge state using an electron obtained from a band edge of the host diamond is less energetically favorable than having the SnV− receive an electron from a neighboring donor dopant. Among donor dopants, substitutional N (NC) is always present in even the purest synthetic or natural diamond sample. The mechanism of electron donation by NC has been proposed by Collins for charging the NV in diamond and it has been used to interpret many experimental results. Therefore, in this paper, we use density functional theory (DFT) to explore the pathways for the formation of the SnV− charge state due to electron donation arising from the presence of NC in the host diamond. Explicitly, defect concentrations are calculated in equilibrium in each of the explored pathways to determine the yield of the SnV− throughout each of the pathways. The importance of our work is to suggest experimental ways of enhancing the yield of charged states like the SnV− in diamond for transformative applications in optoelectronics and quantum information.
The elucidation of the mechanism of SnV− formation in diamond is especially important as the SnV− color center has the potential to be a superior single-photon emitter when compared to the NV and to other Group IV impurity-vacancy color centers in diamond. The typical formation of SnV involves placing Sn in diamond by ion implantation, but the formation of a charged SnV species requires an additional complication. This complication is related to the energy cost associated with electronic transitions within the host diamond. Effectively, producing the SnV− charge state using an electron obtained from a band edge of the host diamond is less energetically favorable than having the SnV− receive an electron from a neighboring donor dopant. Among donor dopants, substitutional N (NC) is always present in even the purest synthetic or natural diamond sample. The mechanism of electron donation by NC has been proposed by Collins for charging the NV in diamond and it has been used to interpret many experimental results. Therefore, in this paper, we use density functional theory (DFT) to explore the pathways for the formation of the SnV− charge state due to electron donation arising from the presence of NC in the host diamond. Explicitly, defect concentrations are calculated in equilibrium in each of the explored pathways to determine the yield of the SnV− throughout each of the pathways. The importance of our work is to suggest experimental ways of enhancing the yield of charged states like the SnV− in diamond for transformative applications in optoelectronics and quantum information.
Experiments with the negatively charged nitrogen vacancy (NV−) in diamond highlight this defect's promise for coherent storage of quantum information. They have also spurred investigations of other color centers in diamond formed by defects that consist of Group IV element (Si, Ge, Sn, Pb) and vacancies which have different atomic structure than the NV− center. To date, these other color centers have not exhibited coherence quite as impressive as that of the NV− center. Spectral diffusion and the low Debye-Waller factor are important limitations of the NV− center that make investigation of the other color centers necessary to advance the field. In this work we use density-functional theory (DFT) to study the thermodynamics and kinetics associated with the NV, SiV, GeV, SnV and PbV color centers in diamond. We find agreement between our theoretical calculations and the charge state of various color centers as observed in intrinsic diamond. We determine the Fermi level values that enhance the production of isolated color centers, which may lead to longer coherence times than their present values.
Tin-vacancy (SnV) and other group-IV vacancy centers in diamond (SiV, GeV, and PbV) are intensively studied as promising alternatives to the nitrogen-vacancy (NV) center for quantum-based applications. The knowledge and the control of their charge state are therefore major issues. Here, using p-i-p planar junctions, we explore the charge states of implanted single SnV centers. We find two classes of centers, emitting either at 620 nm (SnV – ) or at 646.8 nm but not both. We demonstrate the active and reversible tuning of individual SnV – centers. However, unlike the NV centers, which we tune reversibly and continuously between NV – (638 nm), NV 0 (575 nm), and NV + (dark) states, the two kinds of SnV centers do not tune from one to the other. These findings indicate that the 646.8 nm line is likely owing to another Sn-related defect rather than to the neutral charge state of the split vacancy SnV defect along the ⟨111⟩ axis. Furthermore, p-i-p structures can be used efficiently to induce a tunable band bending, stabilize SnV – and NV – states, and explore the charge-state transition energies of many defect centers.
The nitrogen-vacancy (NV) lattice defect in diamond, consisting of an N substitutional atom and an adjacent C vacancy, is commonly observed in two charge states, negative (NV−) and neutral (NV0). The NV− defect exhibits spin state-dependent fluorescence and is, therefore, amenable to optical methods for spin-state readout, while the NV0 is not. Hence, the NV− defect is much more useful for quantum sensing and quantum information processing. However, only NV0 electroluminescence has been observed, even from centers showing NV− in photoluminescence. In the present work, we use first-principles electronic structure calculations to determine adiabatic charge transition levels for the conversion of NV− to NV0 in the presence of substitutional N or P impurities, which provide the charge of the NV− center. We find that the adiabatic charge transition levels in the presence of such impurities lie at energies close to or lower than the zero-phonon line of the NV− center and that these energies only decrease as the concentration of N donors increases. This work, therefore, elucidates the absence of observed electroluminescence from the NV− and proposes a path toward observation of the phenomenon.
Group IV color centers in diamond have garnered great interest for their potential as optically active solid-state spin qubits. The future utilization of such emitters requires the development of precise site-controlled emitter generation techniques that are compatible with high-quality nanophotonic devices. This task is more challenging for color centers with large group IV impurity atoms, which are otherwise promising because of their predicted long spin coherence times without a dilution refrigerator. For example, when applied to the negatively charged tin-vacancy (SnV – ) center, conventional site-controlled color center generation methods either damage the diamond surface or yield bulk spectra with unexplained features. Here we demonstrate a novel method to generate site-controlled SnV – centers with clean bulk spectra. We shallowly implant Sn ions through a thin implantation mask and subsequently grow a layer of diamond via chemical vapor deposition. This method can be extended to other color centers and integrated with quantum nanophotonic device fabrication.
Diamond has been extensively examined as an appealing material for use in quantum optics and quantum information processing owing to the existence of various classes of optically active defects, referred to as “color centers,” which can be engineered into its crystal structure. Among these defects, the negatively charged nitrogen-vacancy center (NV−) stands out as the most prominent type. Despite the progress made, the number of emitters characterized by reproducible fabrication processes within the desired spectral range at room temperature, with limited or no damage to the parent diamond lattice, remains restricted. Herein, we are proposing for the first time the creation of the FV− center in diamond via low-energy implantation, which is particularly interesting as it possesses characteristic light absorption and magnetic properties similar to NV− centers. The low-energy ion-implanted FV centers in diamond show more desirable optical emission properties at room temperature (RT). Additionally, as per DFT calculations, the flat bands near the Fermi energy indicate dominant electron–electron interactions, an important prerequisite for observing emergent behavior as seen in systems such as twisted bi-layer graphene. Consequently, as-developed new luminescent defects such as Fluorine Vacancy Centers (FV) with desirable spectral and quantum emission properties would be a significant breakthrough in diamond-based quantum materials.
The charge state stability of nitrogen-vacancy (NV) centers critically affects their application as quantum sensors and qubits. Understanding charge state conversion and equilibration is important not only for NV centers in diamond but also for defects and impurities in wide-bandgap materials in general. The mechanisms by which these centers change charge state upon optical or electronic excitation without the presence of mobile carriers remain unclear. Here, we elucidate this issue for the case of photoionization of NV center ensembles. Using pump-probe spectroscopy, we ionize negatively charged NV centers and monitor the recovery of NV^{-} on timescales of up to several seconds. We find that the recovery rate depends strongly on the concentration of surrounding nitrogen donors. Remarkably, the equilibration dynamics exhibit no discernible dependence on temperature, ruling out thermally activated processes. We develop a multiphonon-assisted electron-tunneling model, supported by density-functional calculations, that explains the measurements and identifies tunneling as the equilibration mechanism. Because tunneling rates depend exponentially on donor separation, the random distribution of nitrogen donors spreads recovery times from nanoseconds to hours or longer.