arXiv:1405.5837 · Physical Review B
Isotopic identification of engineered nitrogen-vacancy spin qubits in ultrapure diamond
Takashi Yamamoto, Shinobu Onoda, Takeshi Ohshima, Tokuyuki Teraji, Kenji Watanabe, Satoshi Koizumi, Takahide Umeda, Liam Paul McGuinness, Christoph Müller, Boris Naydenov, Florian Dolde, Helmut Fedder, Jan Honert, Matthew Markham, Daniel J. Twitchen, Jörg Wrachtrup, Fedor Jelezko, Junichi Isoya
Abstract
Nitrogen impurities help to stabilize the negatively-charged-state of ${\mathrm{NV}}^{\ensuremath{-}}$ in diamond, whereas magnetic fluctuations from nitrogen spins lead to decoherence of ${\mathrm{NV}}^{\ensuremath{-}}$ qubits. It is not known what donor concentration optimizes these conflicting requirements. Here we used 10-MeV ${}^{15}{\mathrm{N}}^{3+}$ ion implantation to create ${\mathrm{NV}}^{\ensuremath{-}}$ in ultrapure diamond. Optically detected magnetic resonance of single centers revealed a high creation yield of $40\ifmmode\pm\else\textpm\fi{}3%$ from ${}^{15}{\mathrm{N}}^{3+}$ ions and an additional yield of $56\ifmmode\pm\else\textpm\fi{}3%$ from $^{14}\mathrm{N}$ impurities. High-temperature anneal was used to reduce residual defects, and charge stable ${\mathrm{NV}}^{\ensuremath{-}}$, even in a dilute $^{14}\mathrm{N}$ impurity concentration of 0.06 ppb were created with long coherence times.